| MOQ: | 1 Ton |
| Price: | 400-700 USD/Tonc |
| Delivery Period: | 7 - 15 Days |
| Payment Method: | L/C,T/T |
| Supply Capacity: | 20000Tons/Month |
| Performance Indicator | PVDF Fluorocarbon Coating | Ordinary PE Coating | SMP Coating |
|---|---|---|---|
| UV Resistance Lifespan | 20–30 years | 3–5 years | 8–10 years |
| Salt Spray Test Duration | 5000h | 1000h | 2000h |
| Damp Heat Resistance | Excellent | Average | Good |
| Self-Cleaning Function | Yes | No | Weak |
| Application Scenario | Recommended Substrate | Core Advantages |
|---|---|---|
| Coastal high-salt factories/roofing | 275g/m² Hot-Dip Galvanized | High-zinc coating resists salt spray erosion |
| Tropical high-UV building cladding | Hot-Dip Galvalume | Heat/weather resistance reduces fading |
| High-end commercial exterior walls | Galvalume + PVDF Coating | Long-lasting color, self-cleaning, sleek appearance |
| Industrial warehouse partitions | 80g/m² Hot-Dip Galvanized | Cost-effective basic corrosion protection |
|
|
| MOQ: | 1 Ton |
| Price: | 400-700 USD/Tonc |
| Delivery Period: | 7 - 15 Days |
| Payment Method: | L/C,T/T |
| Supply Capacity: | 20000Tons/Month |
| Performance Indicator | PVDF Fluorocarbon Coating | Ordinary PE Coating | SMP Coating |
|---|---|---|---|
| UV Resistance Lifespan | 20–30 years | 3–5 years | 8–10 years |
| Salt Spray Test Duration | 5000h | 1000h | 2000h |
| Damp Heat Resistance | Excellent | Average | Good |
| Self-Cleaning Function | Yes | No | Weak |
| Application Scenario | Recommended Substrate | Core Advantages |
|---|---|---|
| Coastal high-salt factories/roofing | 275g/m² Hot-Dip Galvanized | High-zinc coating resists salt spray erosion |
| Tropical high-UV building cladding | Hot-Dip Galvalume | Heat/weather resistance reduces fading |
| High-end commercial exterior walls | Galvalume + PVDF Coating | Long-lasting color, self-cleaning, sleek appearance |
| Industrial warehouse partitions | 80g/m² Hot-Dip Galvanized | Cost-effective basic corrosion protection |